| ①将所选原资料钢材放入中频电炉熔炼,使钢水温度到达1600-1700℃; ① put the selected raw material steel into medium frequency electric furnace for smelting, so that the temperature of molten steel reaches 1600-1700 ℃; ②将金属模具预加热到800-900℃坚持恒温; ② preheat the metal mould to 800-900 ℃ and keep constant temperature; ③起动离心机,将进程①中钢水写入进程②中预热后金属模具; ③ start the centrifuge, write the steel water in process ① into the metal mold after preheating in process ②; ④铸件天然冷却到800-900℃坚持1-10分钟; ④ natural cooling of casting to 800-900 ℃ for 1-10 minutes; ⑤用水冷却至挨近常温,脱模取出铸件。 ⑤ cool with water to near normal temperature, demould and take out the casting. |
| 上一页 法兰螺栓紧固方法 |
| 下一页 国标法兰可绕行金属软管的安装方法 |